Copper interconnect barrier layer structure and formation method
Abstract
A method for forming a tungsten-containing copper interconnect barrier layer (e.g., a tungsten [W] or tungsten-nitride [W X N] copper interconnect barrier layer) on a substrate with a high (e.g., greater than 30%) sidewall step coverage and ample adhesion to underlying dielectric layers. The method includes first depositing a thin titanium-nitride (TiN) or tantalum nitride (TaN) nucleation layer on the substrate, followed by the formation of a tungsten-containing copper interconnect barrier layer (e.g., a W or W X N copper interconnect barrier layer) overlying the substrate. The tungsten-containing copper interconnect barrier layer can, for example, be formed using a Chemical Vapor Deposition (CVD) technique that employs a fluorine-free tungsten-containing gas (e.g., tungsten hexacarbonyl [W(CO) 6 ]) or a WF 6 -based Atomic Layer Deposition (ALD) technique. The presence of a thin TiN (or TaN) nucleation layer facilitates the formation of a tungsten-containing copper interconnect barrier layer with a sidewall step coverage of greater than 30% and ample adhesion to dielectric layers. A copper interconnect barrier layer structure includes a thin titanium-nitride (TiN) (or tantalum nit
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 103.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for the formation of a copper interconnect barrier layer on a substrate comprising: depositing one of a thin titanium-nitride nucleation layer and a thin tantalum-nitride nucleation layer on the substrate; and forming a tungsten-containing copper interconnect barrier layer overlying the substrate, wherein the forming step uses a Chemical Vapor Deposition (CVD) technique that employs a fluorine-free tungsten-containing gas.
- Claim 2Depends on #1
The method of claim 1 , wherein the forming step uses a CVD technique that employs tungsten hexacarbonyl as the fluorine-free tungsten-containing gas to form the tungsten copper interconnect barrier layer.
- Claim 3Depends on #2
The method of claim 2 , wherein the forming step uses a CVD technique conducted at a temperature in the range of 300° C. to 500° C. and a pressure in the
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 103 total)
References Cited — Backward Prior Art (14)
Non-Patent Literature (5)
- Creighton "Non-selective Tungsten Chemical-vapor Deposition Using Tungsten Hexacarbonyl," Deposition and Growth: Limits for Microelectronics American Institution of Physics Conference Proceedings 167:192-201(1988).
- Kaplan et al. "The Deposition of Molybdenum and Tungsten Films from Vapor Decomposition of Carbonyls," J. Electrochem. Soc. 117:693-700 (1970).
- Kelsey, Jean E., et al., "Low Temperature Metal-Organic Chemical Vapor Deposition of Tungsten Nitride as Diffusion Barrier for Copper Metallization," J. Vac. Sci. Technol. B 17(3), May/Jun. 1999, pp. 1101-1104, 2193 and Fig.
- Kobayashi, Nobuyoshi, et al, "Study on Mechanism of Selective Chemical Vapor Deposition of Tungsten Using In Situ Infrared Spectroscopy and Auger Electron Spectroscopy," J. Appl. Phys. 69 (2), Jan. 15, 1991, pp. 1013-1019.
- Nanda, Arun K., et al., "Characterization of the Nucleation and Growth Process of CVD-W on TiN Substrates," Mat. Res. Soc. Symp. Proc. vol. 382, 1995 Materials Research Society, pp. 401-406.