Pressure sensitive cohesive
Abstract
A pressure sensitive adhesive/cohesive exhibits excellent cohesive body properties, and other desirable features, even when exposed to heat and polysiloxane based lubricants, such as in a laser printer. The formulation comprises 100 parts by weight natural rubber (e.g. electrosterically stabilized natural rubber graft and block terpolymer), and expressed as percentages by weight of the rubber the following components: about 5-35% (e.g. about 28%) acrylate monomer or monomers (such as methyl methacrylate, cyclohexyl methacrylate, benzyl methacrylate, and/or isobornyl methacrylate); about 0.5-8% acrylic acid and/or about 1-10% 4-acetoxystyrene; about 0-20% ethyl hexyl acrylate; about 1-50% (e.g. about 10-30%) finely divided hard particulate material (such as silica gel); 0-50% (preferably about 10-30%) starch; and 0-40% (preferably at least about 5%) carboxylated styrene-butadiene latex, or carboxylated polychloroprene latex, or a styrene-acrylate-acrylonitrile latex, or vinyl-pyridine styrene-butadiene latex, or pre-crosslinked natural rubber latex, or a tackifier, or combinations thereof. The cohesive is coated onto paper and seals to like cohesive upon the application of a force o
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 7.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A pressure sensitive adhesive/cohesive comprising: a modified rubber latex synthesized by at least reacting 100 parts by weight natural rubber with at least one acrylate monomer at about 5-35% by weight of the natural rubber; and a finely divided hard particulate material, having substantially no thermoplasticity, at about 1-50% by weight of the natural rubber.
- Claim 2Depends on #1
A pressure sensitive adhesive/cohesive as recited in claim 1 further comprising acrylic acid at about 0-8% by weight of the natural rubber.
- Claim 3Depends on #1
A pressure sensitive adhesive/cohesive as recited in claim 1 further comprising 4-acetoxystyrene at about 0-10% by weight of the natural rubber.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (7 of 7 total)
References Cited — Backward Prior Art (15)
Non-Patent Literature (1)
- Ishikawa et al, "Poly-Polymerization of Methyl Methacrylate and Styrene with the Use of Natural Latex" Journal of Polymers, 31:12, 733-737 (1974).