Patents
US 6,602,796 B2#61524096 Most CitedExpiredUnited States (USPTO)Utility

Chemical vapor deposition for smooth metal films

1Forward Citations (#61524096 Global)
0.0/yrCitation Velocity (#56819554 Global)
0.75Citation PageRank (#61524096 Global)
24Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method for growing smooth metal films using a first process phase favorable to nucleation, agglomeration and initiation of smooth metal film growth and a second process phase favorable to continued smooth metal film growth, a system for performing the method, and semiconductor devices so produced.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of forming a single element metal film, comprising: depositing a single element metal film by chemical reaction at a first set of process conditions, the first set of process conditions producing a grain size in the single element metal film; allowing for development of a continuous film; and continuing to deposit the single element metal film by chemical reaction, at a second set of process conditions, wherein the second set of process conditions differs from the first set of process conditions, wherein the second set of process conditions preserves the grain size.

  2. Claim 2Depends on #1

    The method of claim 1 wherein depositing the metal film at the first set of process conditions comprises operating at a first temperature, a first pressure and a first oxidizer concentration.

  3. Claim 3Independent Claim

    The method of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
US 4,818,560 AMethod for preparation of multi-layer structure film198934
EP 0,328,507 A1Process for preparing catalysts containing a metal of the platinum group, and uses thereof—23
US 4,871,691 ASelective deposition process of a refractory metal silicide onto silicon areas19896
US 5,017,543 AProcess for the preparation of a dehydrogenation catalyst199110
EP 0,328,507 B1Process for preparing catalysts containing a metal of the platinum group, and uses thereof19911
US 5,147,819 ASemiconductor metallization method199299
US 5,152,805 AM-I-M' device and fabrication method199217
US 5,231,056 ATungsten silicide (WSix) deposition process for semiconductor manufacture1993133
US 5,278,100 AChemical vapor deposition technique for depositing titanium silicide on semiconductor wafers1994107
US 5,384,289 AReductive elimination chemical vapor deposition processes utilizing organometallic precursor compounds in semiconductor wafer processing199550
US 5,558,910 AUniform tungsten silicide films produced by chemical vapor deposition199624
US 5,576,071 AMethod of reducing carbon incorporation into films produced by chemical vapor deposition involving organic precursor compounds199687
EP 0,751,577 A2Method for the formation of thin PtSi layers on a Si substrate—1
US 5,641,545 AMethod to deposit highly conformal CVD films199780
EP 0,751,577 A3Method for the formation of thin PtSi layers on a Si substrate—1
US 5,661,115 AMethod of reducing carbon incorporation into films produced by chemical vapor deposition involving organic precursor compounds199747
US 5,662,788 AMethod for forming a metallization layer199745
US 5,730,835 AFacet etch for improved step coverage of integrated circuit contacts199831
US 5,733,816 AMethod for depositing a tungsten layer on silicon1998130
US 5,736,422 AMethod for depositing a platinum layer on a silicon wafer199837
US 5,741,546 AMethod of depositing titanium nitride films on semiconductor wafers199820
US 5,856,236 AMethod of depositing a smooth conformal aluminum film on a refractory metal nitride layer199937
US 5,874,131 ACVD method for forming metal-containing films199989
US 6,104,049 AFerroelectric memory with ferroelectric thin film having thickness of 90 nanometers or less, and method of making same200044