Method for non-contact stress evaluation of wafer gate dielectric reliability
Abstract
An apparatus and method for evaluating the performance of a test dielectric material for use as a gate dielectric. The method comprises exposing a coated layer of the dielectric to a concentration of atomic hydrogen. The method may comprise (a) measuring an initial value of interface-state density in the test dielectric, (b) exposing the coated test dielectric to a concentration of atomic hydrogen in a remote plasma, and then (c) measuring a post-exposure value of interface-state density in the test dielectric. Steps (b) and (c) may be repeated with incrementally higher concentrations of atomic hydrogen to determine a rate of change in interface-state density value as a function of atomic hydrogen concentration, which may then be related to the projected charge-to-breakdown or time-to-breakdown of the test dielectric layer when the dielectric is used as the gate dielectric. The method may be conducted on a remote-plasma hydrogen exposure apparatus comprising, in series, a source of a mixture of molecular and atomic hydrogen gas; a particle remover adapted to remove energetic, charged particles; a light sink; a hydrogen recombination device; and a wafer exposure chamber.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for evaluating the performance of a test dielectric material for use as a gate dielectric, the method comprising: a) measuring an initial value of interface-state density in said test dielectric; b) exposing said test dielectric material to a concentration of atomic hydrogen via a remote plasma; and c) measuring a post-exposure value of interface-state density in said test dielectric.
- Claim 2Depends on #1
The method of claim 1 further comprising: d) repeating steps (b) and (c) at least one more time with an incrementally higher concentration of atomic hydrogen each time steps (b) and (c) are repeated; and e) determining a rate of change in interface-state density value as a function of atomic hydrogen concentration.
- Claim 3Depends on #2
The method of claim 2 further comprising relating the ra
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (16)
Non-Patent Literature (5)
- "Atomic hydrogen-induced degradation of the Si/SiO2 structure," by E. Cartier et al., Microelectronic Engineering 28, pp. 3-10 (1995).
- "Atomic hydrogen-induced degradation of thin SiO2 gate oxides," by E. Cartier et al., Journal of Non-Crystalline Solids, 187, pp. 244-247 (1995).
- "Atomic hydrogen-induced interface degradation of reoxidized nitrided silicon dioxide on silicon," by E. Cartier et al., Appl. Phys. Lett. 64(7), pp. 901-903 (Feb. 14, 1994).
- "Degradation of thin SiO2 gate oxides of atomic hydrogen," by E. Cartier et al., IBM Technical Disclosure Bulletin 11, pp. 453-454 (Apr. 1990).
- "Elimination and generation of Si-SiO2 interface traps by low temperature hydrogen annealing," by L. D. Thanh et al., J. Electrochem. Soc.: Solid State Science & Tech., pp. 1797-1801 (Jul. 1988).