Copper-alloy foil to be used for suspension member of hard-disc drive

7Forward Citations (#14609795 Global)
0.3/yrCitation Velocity (#25474996 Global)
2.18Citation PageRank (#12643645 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Conductors, which are formed on a suspension member of the hard-disc drive suspension, are subject to thermal expansion and shrinkage during the laminating process with a substrate via a polyimide binder. The tracking width of the suspension member is influenced by the thermal expansion and shrinkage. In order to provide a copper-alloy foil, which can attain improved tracking width, the following ratio of thermal expansion and shrinkage is adjusted in a range of from -0.1 to +0.1%where l0 the length of a specimen before heating at 330° C. for 2 hours, and l is the length of a specimen after heating at 330° C. for 2 hours. DELTA(%) is measured in the direction parallel to the rolling direction.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 7.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A copper-alloy foil to be used for a suspension member of a hard-disc drive, consisting, by mass percentage, of from 1 to 4.8% of Ni, from 0.2 to 1.4% of Si, a ratio of Ni content relative to Si content being adjusted to 2 to 8, a balance being essentially copper and unavoidable impurities, having 650 MPa or more of tensile strength, and including inclusions not exceeding 10 μm in size and fifty or less inclusions from 5 to 10 μm in size per mm 2 of a cross section of the foil in a direction parallel to a rolling direction, and exhibiting from −0.1 to +0.1% of a following ratio of thermal exp