Patents
US 6,599,563 B2#24428055 Most CitedExpiredUnited States (USPTO)Utility

Method and apparatus for improving interfacial chemical reactions in electroless depositions of metals

4Forward Citations (#24428055 Global)
0.2/yrCitation Velocity (#36177797 Global)
1.43Citation PageRank (#24663557 Global)
5Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method and apparatus for improving interfacial chemical reactions in electroless depositions of metals, in which the substrate to be plated is pre-heated prior to its immersion in the various processing solutions that require elevated temperatures, and especially before immersion in the electroless plating solution. The pre-heating is carried out to a temperature that is needed to bring about the desired chemical reaction at the substrate-solution interface, allowing the bath of that process step to operate significantly below the temperature that would have been needed if the panel had not been pre-heated, and below the solution temperature of current practice. According to another aspect of the present invention, the electroless plating apparatus for plating a workpiece operates in a vertical mode and it comprises a heating station, with the panel to be plated returning to the heating station as dictated by the temperature required for a given process step. Alternatively, the heating station is incorporated into the hoist system of such apparatus. In still another aspect of the present invention, the electroless plating apparatus operates in a horizontal mode and comprises at l

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for improving interfacial chemical reactions in electroless deposition of metals on the surface of a workpiece using an electroless plating solution in an electroless plating bath, said method comprising: pre-treating the workpiece by at least one of conditioning, activation and acceleration; and pre-heating the workpiece in a pre-heating bath, for a period of up to approximately 5 minutes, prior to immersion thereof in the electroless plating solution, to a temperature approximately equal to or above the operating temperature of the electroless plating bath, such that the workpiece e

  2. Claim 2Depends on #1

    The method of claim 1 , said method further comprising the step of heating the surface of the workpiece pr

Technical Overview & Description