Patents
US 6,599,332 B2#124618031 Most CitedExpiredUnited States (USPTO)Utility

Process for the production of aluminum hydroxide

0Forward Citations (#124618031 Global)
0.0/yrCitation Velocity (#124618031 Global)
0.56Citation PageRank (#124618031 Global)
5Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Aluminium hydroxide of improved thermal stability is produced by spray-drying of an aqueous slurry of aluminium hydroxide at 400 to 600° C. drying gas temperature. The resulting aluminium hydroxide is suitable as a flame retardant filler in polymeric systems with high processing temperatures. It has a low specific surface area and good rheological properties.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for the production of aluminium hydroxide of improved thermal stability, comprising spray-drying of an aqueous slurry of aluminium hydroxide at a drying gas temperature of 400 to 600° C.

  2. Claim 2Depends on #1

    The process of claim 1 , wherein the drying gas temperature is 450 to 550° C.

  3. Claim 3Depends on #1

    The process of claim 1 , wherein the exit gas temperature from the spray-dryer is 200 to 300° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.