The present invention relates to a method for depositing a parylene polymer barrier coating on a polymeric substrate for improving the chemical resistance of the substrate. The method comprises the steps of thoroughly treating a surface portion of the substrate to remove any contaminants, depositing at least one layer of parylene polymer on the contaminant-free surface portion via chemical vapor deposition, and then annealing each of the at least one layer of parylene polymer for a sufficient time. The present invention also relates to a composition for a barrier coating on a polymeric substrate comprising at least one layer of parylene polymer bonded to the surface of the polymeric substrate. The substrate can be a silicone rubber keypad.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 19.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for depositing a barrier coating on a polymeric substrate, the method comprising the steps of: depositing a first layer of parylene N on a clean surface portion of the polymeric substrate; depositing a second layer of parylene C over said first layer; and annealing by heat each layer in the presence of a vacuum or an inert atmosphere at an annealing temperature for a time sufficient to increase the degree of parylene crystallization and to improve the adherence of the parylene C layer on the substrate and its barrier properties.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the annealing temperature is from about 80 to 220° C. and the time period is from about 12 to 100 hours.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein the annealing temperature is about 120° C. and the time period is about 48