US 6,583,545 B1#91290384 Most CitedExpiredUnited States (USPTO)Utility

Aperture grill material for color picture tube, production method thereof, aperture grill and picture tube

0Forward Citations (#91290384 Global)
0.0/yrCitation Velocity (#91290384 Global)
0.56Citation PageRank (#91290384 Global)
12Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A purpose of the present invention is to provide material of an aperture grille used for a color picture tube having excellent yield strength, excellent high temperature creep strength and excellent magnetic characteristic, material of an aperture grille used for a color picture tube for improving an occurrence of cracking during a hot rolling step, a method for producing these material, an aperture grille and a color picture tube with the aperture grille. After adding nickel of 0.01 to 1.75 wt % to low carbon alloy steel including copper of 0.05 to 2.5 wt % and phosphor of 0.001 to 0.4 wt %, material according to the present invention is cold rolled. Then, a precipitation treatment is processed at a temperature of 300 to 700° C. Alternatively, the material is cold rolled and secondary rolled after passing through an intermediate annealing at a temperature of 500 to 800° C. Then, the precipitation treatment is processed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 0.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An aperture grill in a color picture tube consisting essentially of no more than 0.01 wt % carbon, 0.001-0.4 wt % phosphorus, 0.05-2.5 wt % copper, 0.01-1.75 wt % nickel, no more than 0.5 wt % manganese, no more than 0.3 wt % silicon, no more than 0.05 wt % sulfur, no more than 0.05 wt % nitrogen, with the remainder being substantially entirely Fe.

  2. Claim 2Depends on #1

    The aperture grill according to claim 1 wherein the amount of carbon is no more than about 0.006 wt %, the amount of manganese is no more than about 0.47 wt %, the amount of silica is no more than about 0.02 wt %, the amount of sulfur is no more than about 0.01 wt %, the amount of nitrogen is no more than about 0.002 wt %, the amount of phosphorous is at least 0.15 wt %, and the amount of nickel is about 0.024-1.38 wt %.

  3. Claim 3Independent Claim

    In a color picture tube comprising an

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (2)

  • DialogIP Document, English language Abstract of JP 08-067945 A, published Mar. 12, 1996 to Nisshin Steel Co., Ltd.
  • DialogIP Document, English language Abstract of JP 10-158789, published Jun. 16, 1998 to Nisshin Steel Co., Ltd.