Semiconductor element
Abstract
An AlN film as an underlayer is epitaxially grown on a substrate having a dislocation density of 10 11 /cm 2 or below and a crystallinity of 90 seconds or below in full width at half maximum (FWHM) of an X-ray rocking curve at (002) reflection. Then, on the AlN film an n-GaN film is epitaxially grown as a conductive layer having a dislocation density of 10 10 /cm 2 or below and a crystallinity of 150 seconds or below in full width at half maximum (FWHM) of an X-ray rocking curve at (002) reflection, to fabricate a semiconductor element.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 17.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A semiconductor element, comprising: a substrate; an underlayer, epitaxially grown on said substrate, comprising a first semiconductor nitride including at least elemental Al, said underlayer having a dislocation density of 10 11 /cm 2 or below and a crystallinity of 90 seconds or below in full width at half maximum of an X-ray rocking curve at (002) reflection; and a conductive layer, epitaxially grown on said underlayer, comprising a second semiconductor nitride including at least one element selected from the group consisting of Al, Ga and In, said conductive layer having a dislocation den
- Claim 2Depends on #1
The semiconductor element defined in claim 1 , wherein the A
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗