Semiconductor device manufacturing method including forming FOX with dual oxidation
Abstract
In a method of manufacturing a semiconductor device, there are comprised the steps of forming an oxidation preventing layer on a surface of a semiconductor substrate, forming a first window in the oxidation preventing layer, placing the semiconductor substrate in a first atmosphere in which an oxygen gas and a first amount of a chlorine gas are supplied through and then heating the semiconductor substrate at a first temperature such that a first selective oxide film is to grown by thermally oxidizing the surface of the semiconductor substrate exposed from the first window, forming a second window by patterning the oxidation preventing layer, and placing the semiconductor substrate in a second atmosphere in which the oxygen gas and a second amount, which is larger than the first amount, of the chlorine gas are supplied through and then heating the semiconductor substrate at a second temperature such that a second selective oxide film is formed and that a thickness of the first selective oxide film formed below the first window is enhanced. Accordingly, generation of projection on bird's beak of a selective oxide film can be prevented in a semiconductor device manufacturing metho
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of manufacturing a semiconductor device comprising the steps of: forming an oxidation preventing layer on a surface of a semiconductor substrate; forming a first window by patterning the oxidation preventing layer; placing the semiconductor substrate in a first atmosphere in which an oxygen gas and a first amount of a chlorine or chloride gas are supplied, and then heating the semiconductor substrate at a first temperature such that a first field oxide layer is to grown by thermally oxidizing the surface of the semiconductor substrate exposed from the first window; forming a second wi
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗