Abstract

Modified graphite particles are described, which have an almost circular and tabular shape, an average particle size Ap of 12 to 18 mum, a BET specific surface area Ss of 4 to 6 m2/g, and a BET specific surface area to average particle size ratio, Ss/Ap, of 0.35 or less, and which are obtained by treating tabular particles of lumpy or flaky graphite to break or slightly fold the periphery of the tabular particles to increase the degree of circularity. A battery having the modified graphite particles as an anode active material is also described.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A battery having an anode active material comprising uncoated modified natural or artificial graphite particles having an almost circular and tabular shape, an average particle size Ap of 12 to 18 μm, a BET specific surface area Ss of 4 to 6 m 2 /g, and a BET specific surface area to average particle size ratio, Ss/Ap, of 0.35 or less, said uncoated modified graphite particles obtained by treating tabular particles of natural or artificial flaky graphite to break or slightly fold the periphery of said tabular particles to increase the degree of circularity.

  2. Claim 2Depends on #1

    The battery as claimed in claim 1 , wherein the Ap is 12 to 16 μm.

  3. Claim 3Depends on #1

    The battery as claimed in claim 1 , wherein the Ss is 4 to 5 m 2 /g.