Patents
US 6,571,665 B2#5071887 Most CitedExpiredUnited States (USPTO)Utility

Cutting instruments

18Forward Citations (#5071887 Global)
0.8/yrCitation Velocity (#9626076 Global)
1.63Citation PageRank (#19994313 Global)
3Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A process for making a cutting instrument includes cutting a blank from a plate or strip of Type 60 Nitinol, having a thickness of between 0.005″-0.500″ using an abrasive waterjet, wire electron discharge machining or laser cutting, and grinding top and bottom surfaces of the blank by rotating a grinder having cubic boron nitride or diamond abrasive particles on a cutting surface of said grinder against the knife blank at a surface speed of about 5000 to 7000 surface feet per minute and grinding to a depth of about 0.001 to 0.005 inches per pass to remove material along the blade surface. The surface of the blade is polished to a surface finish smoother than 20 microinches RMS using Turkish emery abrasive grinding/polishing materials on a buffing wheel driven by a high power motor. The blade is then finish polished to a mirror-like luster of 2 microinches RMS or less using a fine diamond buffing compound and a buffing wheel running at about 3000 RPM. An edge is ground into the polished blade blank using an Arkansas stone grinder.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 18.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for producing surface material on a part made of Type 60 Nitinol parent material, said surface material being electrically non-conductive hard lustrous, non-stick and integral with the parent material, said surface material having a color from a group of colors consisting of gold, red/purple, blue, silver, and green, said process comprising: a. polishing said part to a smooth finish; b. heating said part to a temperature of about 400° C.-650° C. in a gaseous atmosphere simulating indoor air at room temperature until said part attains said color; and c. allowing said part to cool slow

  2. Claim 2Depends on #1

    A process as defined in claim 1 , further comprising: d. polishing said cooled part with a fine grit diamond paste on a buffing wheel; and e. repeating st

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗