A method of making a steel sheet for a tension mask, including the steps of: hot rolling a steel consisting essentially of, by weight %, C: less than 0.1%, Si: 0.05% or less, Mn: 0.4 to 2%, P: 0.03% or less, S: 0.03% or less, sol.Al: 0.01% or less, N: 0.010% or more, and the balance of Fe; and annealing the cold rolled steel sheet, followed by a secondary cold rolling at a reduction rate of 35% or higher. The steel sheet produced by this method shows excellent creep resistance during blackening treatment and excellent magnetic shielding property with an anhysteretic permeability of 3400 or more at a DC bias magnetic field of 0.35 Oe, and therefore causes no color-deviation when applied to the tension mask.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 7.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of making a steel sheet for a tension mask, comprising the steps of: hot rolling a steel consisting essentially of, by weight %, C: less than 0.1%, Si: 0.05% or less, Mn: 0.4 to 2%, P: 0.03% or less, S: 0.03% or less, sol.Al: 0.01% or less, N: 0.010% or more, and the balance of Fe; cold rolling the hot rolled steel sheet; and annealing the cold rolled steel sheet, followed by a secondary cold rolling at a reduction rate of 35% or higher.
- Claim 2Depends on #1
The method as set forth in claim 1 , wherein the content of N is 0.012% or more.
- Claim 3Depends on #2
A steel sheet for a tension mask produced by the method as set forth in claim 2 .