Polyarylensulfide, polyarylensulfide resin composition, method for producing polyarylensulfide
Abstract
Provided are a polyarylene sulfide having a chloroform soluble content of at most 0.5% by weight and having an inherent viscosity etainh of from 0.05 to 0.4; a polyarylene sulfide resin composition comprising a polyarylene sulfide and an inorganic filler, of which the chloroform soluble content is at most 0.5% by weight relative to the polyarylene sulfide in the composition; car parts produced through injection molding of the composition; and a method for producing a polyarylene sulfide. The polyarylene sulfide has a reduced content of low-molecular components, and has well balanced properties of fluidity, flexural strength and impact resistance.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 4.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for producing a polyarylene sulfide by reacting a dihalogenaromatic compound with lithium sulfide in an aprotic organic solvent, which is characterized by adding from 21 to 100 mol %, relative to the starting lithium sulfide, of lithium hydroxide to the reaction system.
- Claim 2Depends on #1
The method for producing a polyarylene sulfide as claimed in claim 1 , which is characterized by two-stage polymerization comprising a prepolymerization step of putting a part of the necessary amount of the starting dihalogenaromatic compound into the reaction system and a final polycondensation step of adding the remaining part of the starting dihalogenaromatic compound to the reaction mixture that contains the prepolymer formed in the previous step, or by multi-stage polymerization of repeating the two steps.
- Claim 3Independent Claim
A method for produ