Abstract

Polyurethane elastomers are produced by reacting a polyether and/or polyester polyol having a starter functionality of at least 2 with an NCO-terminated prepolymer produced with a polyether and/or polyester polyol having a starter functionality of at least 4. These polyurethane elastomers exhibit improved processing characteristics combined with a high heat distortion temperature.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 11.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the production of a polyurethane elastomer comprising reacting a) from about 25 to about 50 wt. %, based on total weight of elastomer, of a polyether and/or polyester polyol having a number average molecular weight of from 500 to 18,000 and a starter functionality of at least 2, b) from about 6 to about 14 wt. %, based on total weight of elastomer, of a glycolic chain extender having at least two hydroxyl groups per molecule and a molecular weight of from 62 to 499, and c) from about 0.05 to about 0.5 wt. %, based on total weight of elastomer, of a catalyst with d) an NCO-termina