Patents
US 6,566,478 B1#3615208 Most CitedExpiredUnited States (USPTO)Utility

Synthesis of high vinyl rubber

22Forward Citations (#3615208 Global)
1.0/yrCitation Velocity (#7496954 Global)
4.72Citation PageRank (#3643792 Global)
13Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

This invention is based upon the discovery that rubbery polymers having a high vinyl content and a low degree of branching can be synthesized with an initiator system that is comprised of (a) a lithium initiator selected from the group consisting of allylic lithium compounds and benzylic lithium compounds, (b) a Group I metal alkoxide, and (c) a polar modifier; wherein the molar ratio of the Group I metal alkoxide to the polar modifier is within the range of about 0.1:1 to about 10:1; and wherein the molar ratio of the Group I metal alkoxide to the lithium initiator is within the range of about 0.01:1 to about 20:1. These high vinyl polymers offer reduced levels of hysteresis and better functionalization efficiency. By virtue of their lower level of hysteresis these polymers can be utilized in manufacturing tire tread compounds that exhibit lower levels of rolling resistance and can accordingly be used to improve the fuel economy of motor vehicles without compromising other desirable characteristics, such as traction and tread-wear.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 22.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a rubbery polymer having a high vinyl content which comprises: polymerizing at least one diene monomer with a lithium initiator selected from the group consisting of allylic lithium compounds and benzylic lithium compounds at a temperature which is within the range of about 5° C. to about 120° C. in the presence of a Group I metal alkoxide and a polar modifier, wherein the molar ratio of the Group I metal alkoxide to the polar modifier is within the range of about 0.1:1 to about 10:1; and wherein the molar ratio of the Group I metal alkoxide to the lithium initiator is

  2. Claim 2Independent Claim

    An initiator system which is comprised of (a) a lithium initiator selected from the group consisting of allylic lithium compounds and benzylic lithium compounds, (b) a Group I metal

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗