Abstract
The HF defect density in an SOI is reduced. An SOI having a thickness of 200 nm or less is annealed in an inert atmosphere at a temperature between the eutectic temperature (e.g., 966° C.) of a semiconductor metal compound (e.g., nickel silicide) formed from a metal and the semiconductor material of the crystal semiconductor of the SOI (inclusive) and the melting point of the semiconductor material (inclusive).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 20.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An SOI annealing method comprising: the first annealing step of annealing an SOI having a semiconductor layer with a thickness of not more than 200 nm on an insulator in a first reducing atmosphere at a temperature not more than a melting point of silicon; and the second annealing step of, after the first annealing step, annealing the SOI in an inert atmosphere or a second reducing atmosphere weaker than the first reducing atmosphere at a temperature between 966° C. (inclusive) and the melting point of silicon (inclusive).
- Claim 2Depends on #1
The method according to claim 1 , wherein the annealing temperature in the first annealing step is not less than 775° C.
- Claim 3Depends on #1
The method according to claim 1 , wherein the annealing temperature in the first annealing step is not less than 966° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 20 total)
References Cited — Backward Prior Art (17)
Non-Patent Literature (1)
- Sadana, D.K., et al., Nanodefects in commercial bonded SOI and Simox, Proceedings 1994 IEEE International SOI Conference, Oct. 1994.