Lead free liner composition for shaped charges
Abstract
A liner for a shaped charge formed from a mixture of powdered heavy metal and a powdered metal binder. The liner is formed by compression of the mixture into a liner body shape. In the preferred embodiment of the invention, the mixture comprises a range of 90 to 97 percent by weight of powdered heavy metal, and 10 to 3 percent by weight of the powdered metal binder. In a specific embodiment of the invention, a lubricant is intermixed with the powdered metal binder to aid in the formation of the shaped charge liner. The preferred powdered heavy metal is tungsten, and the preferred powdered metal binder is copper. The powdered metal binder can be comprised of other malleable ductile metals such as bismuth, zinc, tin, uranium, silver, gold, antimony, cobalt, zinc alloys, tin alloys, nickel, or palladium.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 22.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A liner for a shaped charge comprising: a mixture of powdered heavy metal and powdered metal binder wherein said powdered heavy metal comprises from 90 percent by weight of said mixture to 97 percent by weight of said mixture, and wherein said powdered metal binder comprises from 10 percent by weight of said mixture to 3 percent by weight of said mixture, said mixture compressively formed into a liner body shape by cold working under high pressure.
- Claim 2Depends on #1
The liner for a shaped charge of claim 1 further comprising a lubricant intermixed with said tungsten and said powdered metal binder.
- Claim 3Depends on #2
The liner for a shaped charge of claim 2 , wherein said lubricant comprises powdered graphite.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗