Patents
US 6,564,584 B2#12160866 Most CitedExpiredUnited States (USPTO)Utility

Process for manufacturing glass optical elements

9Forward Citations (#12160866 Global)
0.4/yrCitation Velocity (#20851734 Global)
1.61Citation PageRank (#20419235 Global)
23Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Processes for manufacturing glass optical elements by press molding a heated and softened glass material in preheated molds. In the process, the glass material is heated while it is floated by a gas blow and the heated and softened glass material is transferred to the preheated molds and then subjected to press molding. Alternatively, the process comprises: heating a glass material at a temperature at which the glass material has a viscosity of lower than 10 9 poises, preheating molds at a temperature at which the glass material has a viscosity of from 10 9 to 10 12 poises, subjecting the heated and softened glass material to initial press in the preheated molds for 3 to 60 seconds, starting to cool the vicinity of molding surfaces of the molds at a rate of 20° C./minute or higher upon starting of, or during, or after the initial press, and removing a molded glass article from the molds after the temperature of the vicinity of the molding surfaces of the molds becomes a temperature equal to or lower than a temperature at which the glass material has a viscosity of 10 12 poises.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for manufacturing glass optical elements by press molding a preheated and softened glass material in preheated molds with mirror molding surface of a shape corresponding to the shape of an article to be manufactured, which comprises the steps of: a. heating a glass material at a temperature at which the glass material has a viscosity of from 10 5.5 to 10 7.6 poises. b. transferring the heated and softened glass material to molds preheated at a temperature at which the glass material has a viscosity of from 10 9 to 10 12 poises c. subjecting the transferred glass material to press

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗