Method of manufacturing a semiconductor device comprising semiconductor elements formed in a toplayer of a silicon wafer situated on a buried insulating layer

1Forward Citations (#46103272 Global)
0.0/yrCitation Velocity (#55363899 Global)
1.26Citation PageRank (#29886039 Global)
13Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of manufacturing a semiconductor device including semiconductor elements having semiconductor zones ( 17, 18, 24, 44, 45 ) formed in a top layer ( 4 ) of a silicon wafer ( 1 ) situated on a buried insulating layer ( 2 ). In this method, a first series of process steps are carried out, commonly referred to as front-end processing, wherein, inter alia, the silicon wafer is heated to temperatures above 700° C. Subsequently, trenches ( 25 ) are formed in the top layer, which extend as far as the buried insulating layer and do not intersect pn-junctions. After said trenches have been filled with insulating material ( 26, 29 ), the semiconductor device is completed in a second series of process steps, commonly referred to as back-end processing, wherein the temperature of the wafer does not exceed 400° C. The trenches are filled in a deposition process wherein the wafer is heated to a temperature which does not exceed 500° C. In this manner, a semiconductor device can be made comprising semiconductor elements having very small and shallow semiconductor zones.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a semiconductor device comprising semiconductor elements having semiconductor zones formed in a silicon wafer's monocrystalline top layer situated on a buried insulating layer, in which method a first series of process steps is carried out, inter alia, process steps wherein the wafer is heated to a temperature above 700° C., whereafter trenches are formed in the top layer which extend as far as the buried insulating layer and which do not intersect pn-junctions, which trenches are subsequently filled with an insulating material, after which a second series of proc

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

Non-Patent Literature (2)

  • Wolf et al., "Chemical Vapor Deposition of Amorphous and Polycrystalline Films," Silicon Processing for the VLSI Era-vol. 1: Process Technology, Lattice Press (1986), pp. 182-185.
  • Wolf et al., “Chemical Vapor Deposition of Amorphous and Polycrystalline Films,” Silicon Processing for the VLSI Era—vol. 1: Process Technology, Lattice Press (1986), pp. 182-185.