Abstract
A steel sheet for heat shrink band of the present invention has anhysteretic magnetic permeability of 15,000 or higher at 0.35 Oe and yield stress of 24 kgf/mm2 or more. The steel sheet can be manufactured by a method comprising the steps of: hot rolling and/or cold rolling a steel containing 0.01 to 0.15% C by weight; annealing the rolled steel sheet at a temperature ranging from 650 to 900° C.; and temper rolling the annealed steel sheet at a rolling reduction rate of 1.5% or less. A CRT made of the steel sheet causes very little color deviation and practically no deformation of the panel surface.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 3.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A steel sheet for heat shrink band, having anhysteretic magnetic permeability of 15,000 or higher at 0.35 Oe and yield stress of 24 kgf/mm 2 or more.
- Claim 2Depends on #1
The steel sheet for heat shrink band of claim 1 , wherein coercive force thereof is 5 Oe or less and remanent magnetic flux density is 10 kG or larger.
- Claim 3Depends on #1
The steel sheet for heat shrink band of claim 1 , containing 0.01 to 0.15% C by weight.