Patents
US 6,558,517 B2#12202283 Most CitedExpiredUnited States (USPTO)Utility

Physical vapor deposition methods

9Forward Citations (#12202283 Global)
0.4/yrCitation Velocity (#20857248 Global)
1.55Citation PageRank (#21652964 Global)
33Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The invention includes chemical vapor deposition and physical vapor deposition methods of forming high k ABO3 comprising dielectric layers on a substrate, where "A" is selected from the group consisting of Group IIA and Group IVB elements and mixtures thereof, and where "B" is selected from the group consisting of Group IVA metal elements and mixtures thereof. In one implementation, a plurality of precursors comprising A, B and O are fed to a chemical vapor deposition chamber having a substrate positioned therein under conditions effective to deposit a high k ABO3 comprising dielectric layer over the substrate. During the feeding, pressure within the chamber is varied effective to produce different concentrations of A at different elevations in the deposited layer and where higher comparative pressure produces greater concentration of B in the deposited layer. In one implementation, a subatmospheric physical vapor deposition method of forming a high k ABO3 comprising dielectric layer on a substrate includes providing a sputtering target comprising ABO3 and a substrate to be deposited upon within a physical vapor deposition chamber. A sputtering gas is fed to the cha

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 33 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A subatmospheric pressure physical vapor deposition method of forming a high k ABO 3 comprising dielectric layer on a substrate, where “A” is selected from the group consisting of Sn and Group IIA metal elements and mixtures thereof, where “B” is selected from the group consisting of Group IVA elements and mixtures thereof, the method comprising: providing a sputtering target comprising ABO 3 and a substrate to be deposited upon within a physical vapor deposition chamber; feeding a sputtering gas to the chamber under conditions effective to sputter the target and deposit a high k ABO 3 comp

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (33)

PatentTitleYearCitations
EP 0,474,140 A1Process of forming capacitive insulating film—26
US 5,254,505 AProcess of forming capacitive insulating film199358
US 5,256,455 AMethod of forming film of tantalum oxide by plasma chemical vapor deposition199338
US 5,459,635 ALaminated thin film capacitor and method for producing the same199547
US 5,470,398 ADielectric thin film and method of manufacturing same199550
US 5,596,214 ANon-volatile semiconductor memory device having a metal-insulator-semiconductor gate structure and method for fabricating the same1997130
US 5,618,761 AMethod of manufacturing a perovskite thin film dielectric1997171
US 5,731,948 AHigh energy density capacitor199871
US 5,776,254 AApparatus for forming thin film by chemical vapor deposition1998128
US 5,783,253 AMethod for forming a dielectric film and method for fabricating a capacitor using the same199872
EP 0,855,735 A2A high temperature, high flow rate chemical vapor deposition apparatus and related methods—31
US 5,798,903 AElectrode structure for ferroelectric capacitor integrated on silicon1998156
WO 9,839,497 A1Deposition of thin films—25
US 5,834,060 AHigh dielectric constant thin film structure method for forming high dielectric constant thin film and apparatus for forming high dielectric contact thin film199850
US 5,972,430 ADigital chemical vapor deposition (CVD) method for forming a multi-component oxide layer1999245
EP 0,957,522 A2Semiconductor memory device and method for fabricating the same—10
WO 9,964,645 A1A method and apparatus for the formation of dielectric layers—18
US 6,037,205 AMethod of forming capacitor for semiconductor device using N2 O gas200033
US 6,043,526 ASemiconductor memory cell using a ferroelectric thin film and a method for fabricating it2000122
US 6,046,345 ABarium strontium β-diketonates, processes for producing the same and processes for producing barium strontium-containing oxide dielectric films with the use of the same200018
US 6,078,492 AStructure of a capacitor in a semiconductor device having a self align contact window which has a slanted sidewall200050

Non-Patent Literature (5)

  • Arai T. et al., Preparation of SrTiO3 Films on 8-Inch Wafers by Chemical Vapor Deposition, 35 JPN. J. Appl. Phys., Part 1, No. 9B, pp. 4875-4879 (Sep., 1996).
  • Basceri C. "Electrical and Dielectric Properties of (Ba,Sr)TiO3 Thin Film Capacitors for Ultra-High Density Dynamic Random Access Memories", 1997, dissertation submitted to Graduate Faculty of N. Carolina State Univ., Dept. Of Materials Science and Engineering.
  • Basceri et al.; "The dielectric response as a function of temperature and film thickness . . . " American Institute of Physics, Sept. 1, 1997, vol. 82, No. 5, pp. 2497-2504.
  • Chung Ming Chu et al., Abstract, Electrical properties and crystal structure of (Ba,Sr)TiO3 films prepared at low temperatures on a LaNiO3 electrode by radio-frequency magnetron. . . , 70 Applied Physics Letters No. 2, pp. 249-251 (1997).
  • H. Yamaguchi, et al., Abstract, Reactive coevaporation synthesis and characterization of SrTiO3-BaTiO3 thin films, IEEE International Symposium on Applications of Ferroelectrics, Greenville, SC, pp. 285-288 (Aug. 2, 1992).