Method for pressing oxynitride glass, disk of oxynitride glass made by said method, and pressing die for said method
Abstract
A method of producing a disk having a radius of r and a thickness of 2h from an oxynitride glass by pressing, said method being characterized in that the pressing load (F), the pressing temperature (T), and the pressing time (t) are defined by the expression below. 1900 ≥ T ≥ 100 × log 10 ( 0.045 × π × r 4 t × h 2 × F ) + A ( 1 ) where, F: pressing load (N) T: pressing temperature (° C.) t: pressing time (s) π: ratio of the circumference to its diameter r: radius of disk formed by pressing (mm) h: half a thickness of disk formed by pressing (mm) A: constant depending on glass composition (° C.) defined by 1450° C.≦A≦650° C. According to this method, it is possible to establish the optimum conditions for making disks from oxynitride glass, and it is possible to provide disks of oxynitride glass suitable for use as high-performance magnetic disk having a high specific rigidity.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 8.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of producing a disk having a radius of r and a thickness of 2h from an oxynitride glass by pressing method, wherein in the method the pressing load (F), the pressing temperature (T), and the pressing time (t) are defined by the expression below: 1900 ≥ T ≥ 100 × log 10 ( 0.045 × π × r 4 t × h 2 × F ) + A ( 1 ) where, F: pressing load (N) T: pressing temperature (° C.) t: pressing time (s) π: ratio of the circumference to its diameter r: radius of disk formed by pressing
- Claim 2Independent Claim
A meth
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.