US 6,553,170 B2#2505524 Most CitedExpiredUnited States (USPTO)Utility

Method and system for a combination of high boron and low boron BPSG top clad fabrication process for a planar lightwave circuit

28Forward Citations (#2505524 Global)
1.2/yrCitation Velocity (#4921404 Global)
5.57Citation PageRank (#2777767 Global)
23Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of depositing a dual layer top clad for an optical waveguide of a planar lightwave circuit (PLC). The method includes a first step of providing a high flow rate of a Boron dopant gas for a first top cladding layer deposition process. Then, a low flow rate of a Boron dopant gas is provided for a second top cladding layer deposition process. The second top cladding layer deposition process is performed directly on the first top cladding layer deposition. The first and second top cladding layer deposition processes are combined to form a dual layer top clad of the PLC having a high Boron portion covering a plurality of optical cores and a low Boron portion covering the first portion. The first top cladding layer deposition process can comprises three deposition and anneal cycles using the high flow rate for the Boron dopant gas. The three deposition and anneal cycles are used to fill gaps between the plurality of optical cores of the PLC. The second top cladding layer deposition process comprises a single deposition and anneal cycle using the low flow rate for the Boron dopant gas. The low Boron portion is configured to cover the high Boron portion and protect the high Boron

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 28.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of depositing a top clad layer for an optical waveguide of a planar lightwave circuit (PLC), the method comprising the steps of: a) providing a high flow rate of a Boron dopant gas for a first top cladding layer deposition process; and b) providing a low flow rate of a Boron dopant gas for a second top cladding layer deposition process, the first top cladding layer and the second top cladding layer combined to form a top cladding layer of the PLC having a high Boron portion covering a plurality of optical cores and a low Boron portion covering the high Boron portion.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the first top cladding layer deposition process comprises three deposition and anneal cycles using the high flow rate for the Boron dopant gas.

  3. Claim 3Depends on #2

    The method of claim 2 wherein the thr