Polymer films and a process for the production thereof
Abstract
The present invention concerns a polyethylene composition particularly suitable for film blowing. The invention also concerns a process for the production thereof. The composition comprises a low molecular weight portion having a density of more than 960 kg/m 3 and a high molecular weight portion. The polyethylene composition has a density of about 925-940 kg/m 3 and a melt flow rate in the range of MFR 21 , from 5 to 40 g/10 min. A polyethylene film blown from the polyethylene composition exhibits a tensile strength at yield in transverse direction at least 15 MPa, a 1% secant modulus in machine direction at least 300 MPa and in transverse direction at least 400 MPa, and a dart drop of at least 5 g/μm.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 25.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A blown polyethylene film comprising a polyethylene composition having (i) a low molecular weight portion having a density of more than 960 kg/m 3 and an MFR 2 higher than 100 g/10 min; and (ii) a high molecular weight portion which has an MFR 21 of less than 50 g/10 min, the polyethylene composition having a density between 929-934 kg/m 3 and MFR 2 , between 12-30 g/10 min and said film exhibiting tensile strength, in transverse direction of at least 15 MPa;, 1% secant modulus in machine direction of at least 300 MPa and in transverse direction of at least 400 MPa; and, when run to a film
- Claim 2Independent Claim
A blown polyethylene film comprising a polyethylene composition having
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗