Propylene terpolymers
Abstract
A process for producing terpolymers of propylene, comprising a) feeding into a slurry reactor a reaction mixture containing 50-85 w-% of propylene, 1-10 w-% of ethylene, 15-40 w-% of another C 4 -C 8 alpha-olefin, a catalyst system maintaining olefin polymerization at said temperature conditions, and optionally hydrogen, b) polymerizing said reaction mixture at a temperature of lower than 70° C. a sufficient time to obtain a propylene terpolymer amounting to 50-99 w-% of the end product, c) transferring said reaction mixture into a gas phase reactor operating at a pressure of higher than 5 bars, preferably higher than 10 bars, optionally adding 0-30 w-% of ethylene, 0-10 w-% of another C 4 -C 8 alpha-olefin, 0-40 w-% of propylene and optionally hydrogen, and d) continuing polymerization in said gas phase reactor for obtaining a propylene terpolymer amounting to 1-50 wt-% of the end product. The terpolymer has a melting temperature a less than 135° C., preferably less than 132° C., and it can be used for manufacturing films having good sealing properties.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 4.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A film-making terpolymer of propylene, comprising a mixture of different propylene terpolymer compositions and further comprising comonomer units derived from ethylene and at least one alpha-olefin selected from the group of C 4 -C 8 alpha-olefins, the weight ratio of ethylene to the C 4 -C 8 alpha-olefin(s) being less than 0.3 and the hexane solubles fraction is less than 6.5% calculated from the total weight of the terpolymer.
- Claim 2Depends on #1
The terpolymer according to claim 1 , comprising 0.3 to 3 wt-% units derived from ethylene and 1 to 15 wt-% units derived from at least one C 4 -C 8 alpha-olefin.
- Claim 3Depends on #1, #2
The terpolymer according to claim 1 or claim 2 , having a melting temperature of about 132° C. or 126° C., wherein the fraction of polymer, determined by DSC, melting below 120° C. or 110° C., respectively, is gre
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (2)
- Front page of FI 70028 corresponds to EP 0 045 975 A2 (no month, year).
- Front page of FI 88047 corresponds to WO 92/19653 (no month, year).