Procedure for the thermal treatment of rails
Abstract
A method for the thermal treatment of rails, in particular of the rail head, in which cooling is carried out in a cooling agent that contains a synthetic cooling agent additive starting at temperatures above 720° C. The treatment is carried out by immersion in the cooling agent until withdrawal of the immersed areas occurs, at a surface temperature between 450 and 550° C. results without temperature equalization across the whole of the cross-section, thereby avoiding hardening of the rail web whilst maintaining an optimal cooling rate for the rail head.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 4.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for the thermal treatment of a rail head of a rail wherein cooling is carried out, comprising: partially submerging the rail by immersing the nil head at an initial temperature of above 720° C. in a cooling agent that contains a synthetic cooling agent additive; and withdrawing the immersed rail head from the cooling agent upon obtaining a surface temperature of the rail head of between 450 and 550° C.; wherein the rail bead includes an inner portion and an outer portion, the outer portion being closer to a surface of the rail head than the inner portion, and wherein the rail head is
- Claim 2Depends on #1
A method set forth in claim 1 , wherein the sy
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗