Ladle refining of steel

20Forward Citations (#4176941 Global)
0.9/yrCitation Velocity (#8314401 Global)
3.96Citation PageRank (#4843393 Global)
20Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A steel charge and slag forming material is heated in a ladle to form molten steel covered by a slag containing silicon, manganese and calcium oxides. The steel is stirred by injection of an inert gas such as argon or nitrogen to cause silicon/manganese-deoxidation and desulphurization to produce a silicon/manganese killed molten steel. Stirring of the molten steel by the inert gas injection while in contact with slag high in calcium oxide generates low free oxygen levels in the steel and desulphurization to sulphur levels below 0.009%. The slag may subsequently be thickened by lime addition to prevent reversion of sulphur back into the steel and oxygen may be injected into the steel to increase its free oxygen content to produce a steel that is readily castable in a twin roll caster.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 20.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of refining steel in a ladle, including heating a steel charge and slag forming material in a ladle to form molten steel covered by a slag containing silicon, manganese and calcium oxides, wherein the molten steel has a carbon content in the range 0.001% to 0.1% by weight, a manganese content in the range of 0.1% to 2.0% by weight and a silicon content in the range 0.1% to 10% by weight, and stirring the molten steel by injecting an inert gas into it to cause silicon/manganese deoxidation and desulphuization of the steel to produce a silicon/manganese killed molten steel having a sulp

  2. Claim 2Depends on #1

    The method as claimed in claim 1 wherein the molten has a free oxygen content of no more than 20 ppm during the desulphurization.

  3. Claim 3Depends on #2

    The method as claimed in claim 2 , wherei

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Unit Conversion Chart for gases, http://user.chollian.net~kiam4904/chart.html.
  • Unit Conversion Chart for gases, http://user.chollian.net˜kiam4904/chart.html.