Method of forming a ruthenium film by CVD

5Forward Citations (#19357114 Global)
0.2/yrCitation Velocity (#31162787 Global)
2.20Citation PageRank (#12481530 Global)
9Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

There is provided a technique for forming an Ru film on the bottom of a deep hole with a considerable film thickness for the lower electrode of an information storage capacity element in order to improve the yield of manufacturing DRAMs. The Ru film is formed on the side wall and the bottom of a deep hole as material for preparing the lower electrode of an information storage capacity element to be produced there under the condition of a gasification flow rate ratio of the raw materials ((Ru(C 2 H 5 C 5 H 4 ) 2 /O 2 ) is not less than 10% Then, the ratio of the film thickness of the Ru film on the bottom “b” of the hole to the largest film thickness “a” of the Ru film in the hole is not less than 50%.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 5.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for manufacturing a semiconductor integrated circuit device, comprising: (a) forming an interlayer insulating film over a semiconductor substrate; (b) forming a hole in said interlayer insulating film; (c) forming a first electrically conductive film over a side wall and a bottom of said hole by reacting an organic compound of material of said first electrically conductive film and an oxidizing agent, a gasification flow rate of said organic compound of material of said first electrically conductive film being not less than 5% of a flow rate of the oxidizing agent; (d) forming an ins

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein a depth of sa