Device including an epitaxial nickel silicide on (100) Si or stable nickel silicide on amorphous Si and a method of fabricating the same
Abstract
An integrated circuit device, and a method of manufacturing the same, comprises an epitaxial nickel silicide on (100) Si, or a stable nickel silicide on amorphous Si, fabricated with a cobalt interlayer. In one embodiment the method comprises depositing a cobalt (Co) interface layer between the Ni and Si layers prior to the silicidation reaction. The cobalt interlayer regulates the flux of the Ni atoms through the cobalt/nickel/silicon alloy layer formed from the reaction of the cobalt interlayer with the nickel and the silicon so that the Ni atoms reach the Si interface at a similar rate, i.e., without any orientation preference, so as to form a uniform layer of nickel silicide. The nickel silicide may be annealed to form a uniform crystalline nickel disilicide. Accordingly, a single crystal nickel silicide on (100) Si or on amorphous Si is achieved wherein the nickel silicide has improved stability and may be utilized in ultra-shallow junction devices.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 27.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A microelectronic device comprising: a silicon substrate; and a nickel silicide positioned on said silicon substrate, wherein said nickel silicide includes cobalt therein, and wherein said cobalt comprises a cobalt atomic percentage in a range of two to fifteen percent in said nickel silicide.
- Claim 2Depends on #1
The device of claim 1 wherein said device is a junction chosen from the group consisting of a P+/N junction and a N+/P junction.
- Claim 3Depends on #1
The device of claim 1 wherein said device has a sheet resistance of no more than nine ohm/square, as measured across an area of 100 μm×100 μm at |3V|, after annealing of the device for at least thirty minutes at a temperature of at least 600 degrees Celsius.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 27 total)
References Cited — Backward Prior Art (3)
Non-Patent Literature (5)
- Chiu, K.C.R., Interface and Surface Structure of Epitaxial NiSi2 films, Appl. Phys. Lett. 38, 988, 1981.
- Colgan, E.G., Nickel Silicide Thermal Stability on Polycrystalline and Single Crystalline Silicon, Materials Chemistry and Physics, 46, 209, 1996.
- Julies, B.A., A Study of the NiSi to NiSi2 Transition in the Ni-Si Binary System, Thin Solid Films, 347, 201, 1999.
- Lin, X.W., Integration of NiSi Salicide for Deep Submicron CMOS Technologies, Advanced Interconnects and Contact Materials and Processes for Future Integrated Circuits Symposium 179, 1998.
- Liu, J.F., Improvement of the Thermal Stability of NiSi Films by Using a thin Pt Interlayer, Appl. Phys. Lett. 77.14, 2177, 2000.