Patents
US 6,534,869 B2#37250059 Most CitedExpiredUnited States (USPTO)Utility

Method for reducing stress-induced voids for 0.25 μm micron and smaller semiconductor chip technology by annealing interconnect lines prior to ILD deposition and semiconductor chip made thereby

2Forward Citations (#37250059 Global)
0.1/yrCitation Velocity (#46978026 Global)
1.12Citation PageRank (#35802644 Global)
8Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for making 0.25-micron semiconductor chips includes annealing the metal interconnect lines prior to depositing an inter-layer dielectric (ILD) between the lines. During annealing, an alloy of aluminum and titanium forms first, which subsequently volumetrically contracts, thereby forming a titanium aluminide compound, with the contraction being absorbed by the aluminum. Because the alloy is reacted to form the metal compound prior to ILD deposition, however, the aluminum is not constrained by the ILD when it attempts to absorb the contraction of the alloy. Consequently, the likelihood of undesirable void formation in the interconnect lines is reduced.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A semiconductor chip, comprising: a semiconductor substrate; at least one predetermined pattern of aluminum (Al) lines supported by the substrate, the lines having a reduced void-content, adjacent lines being separated by distances equal to or less than about three-eighths of a micron, at least one line of the pattern comprising a stack, the stack comprising at least one first type layer comprising aluminum (Al), and at least one second type layer comprising titanium (Ti); and at least one intermetallic layer sandwiched between the at least one first type layer and the at least one second type

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

Non-Patent Literature (1)

  • Kikkawa et al, "A quarter-micrometer interconnection technolgy using a TiN/Al-Si-Cu/TiN/Al-Si-Cu/TiN/Ti multilayer structure" IEEE Transactions on Electronic Devices, vol. 40, No. 2, Feb. 1993.