Abstract

The invention presents a deposition method which varies the growth conditions of a film on a patterned substrate. For example, deposition conditions required for obtaining growth are determined for each of the substrate's component surfaces. Film deposition begins under the conditions used to deposit material on one of the substrate materials. Then, the growth parameters are adjusted towards desired conditions for the other substrate material as another small amount of material is deposited. The adjustment and subsequent deposition is repeated until the desired conditions for growth on the second material are met. Growth of the remainder of the film then continues under the desired deposition conditions for growth on the second material.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 12.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of depositing film layers, comprising: providing a substrate composed of first and second materials; determining a growth condition for each of said first and second materials; and depositing at least one film layer onto said first and second materials under a deposition condition that is based initially on the growth condition determined for said first material, wherein the deposition condition is thereafter adjusted based in part on the growth condition determined for said second component material in order to alleviate stress induced during the depositing step.

  2. Claim 2Depends on #1

    The method of claim 1 , further comprising the steps of refining adjustments to the deposition condition until the deposition condition is based only on the growth condition determined for the second material; and

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 2,303,457 ASeries speed-control units194210
US 3,958,263 AStress reduction in algaas-algaasp multilayer structures197642
US 4,048,438 AConductor patterned substrate providing stress release during direct attachment of integrated circuit chips197783
US 4,502,932 AAcoustic resonator and method of making same198589
US 4,556,812 AAcoustic resonator with Al electrodes on an AlN layer and using a GaAs substrate198569
US 4,606,936 AStress free dielectric isolation technology19865
US 4,719,383 APiezoelectric shear wave resonator and method of making same1988212
US 4,719,155 AEpitaxial layer structure grown on graded substrate and method of growing the same198830
US 4,890,370 AManufacturing method for integrated resonator199045
US 4,950,558 AOxidation resistant high temperature thermal cycling resistant coatings on silicon-based substrates and process for the production thereof199097
US 4,988,957 AElectronically-tuned thin-film resonator/filter controlled oscillator199154
US 5,035,923 AProcess for the deposition of high temperature stress and oxidation resistant coatings on silicon-based substrates199126
US 5,061,574 AThick, low-stress films, and coated substrates formed therefrom199127
US 5,075,641 AHigh frequency oscillator comprising cointegrated thin film resonator and active device1991172
US 5,156,909 AThick, low-stress films, and coated substrates formed therefrom, and methods for making same199210
US 5,166,646 AIntegrated tunable resonators for use in oscillators and filters1992149
US 5,185,589 AMicrowave film bulk acoustic resonator and manifolded filter bank1993173
US 5,185,689 ACapacitor having a ruthenate electrode and method of formation1993120

Non-Patent Literature (5)

  • Finot, A., et al.; Small and Large Deformation of Thick and Thin-Film Multi-Layers: Effects of Layer Geometry, Plasticity and Compositional Gradients, 1996, pp. 683-721, J. Mech. Phys. Solids vol. 44, No. 5.
  • IBM ("Voidless Final Closure Process for Polysilicon Trench", vol. 28, No. 10, Mar. 1986).*
  • Kesler, O., et al.; Determination of Processing-Induced Stresses and Properties of Layered and Graded Coatings: Experimental Method and Results for Plasma-Sprayed Ni-Al2O3, 1997, pp. 3123-3134, Acta mater, vol. 45, No. 8.
  • Makhele, L, et al.; Inhibition of Stress corrosion Cracking Using Ion Implantation, Jul., 1996, Abstracts of 41st Annual Conference of the South African Institute of Physics at University of Pretoria.
  • Manuel, P.N., et al.; Residual Stress in SiO2 Film, Jul., 1996, Abstracts of 41st Annual Conference of the South African Institute of Physics at University of Pretoria.