US 6,524,399 B1#45236905 Most CitedExpiredUnited States (USPTO)Utility

Magnetic material

2Forward Citations (#45236905 Global)
0.1/yrCitation Velocity (#47336130 Global)
0.87Citation PageRank (#49572432 Global)
21Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Magnetic materials having a coercivity not less than about 1000 Oersted are prepared in a single step procedure. A molten mixture of a desired composition having a relatively high boron content is cooled at a rate slower than about 105 degrees Celsius per second. Preferably, the molten mixture is cooled by depositing it on a chilled surface such that it forms a layer between about 120 and about 300, and preferably between about 120 and about 150, microns thick.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 2.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    The method of producing a magnetic material comprising the steps of: providing a molten mixture including boron, one or more rare earths and one or more transition metals; and cooling said mixture at a rate slower than about 10 5 degrees Celsius per second and faster than about 10 4 Celsius per second, the molten mixture containing not less than about ten atomic percent boron, not less than about 60 atomic percent transition metals, and not more than about 10 atomic percent rare earths, wherein at least about 90 percent by weight of said rare earths comprise Nd, Pr, or a mixture thereof.

  2. Claim 2Depends on #1

    The method of claim 1 wherein said molten mixture is cooled by impinging said molten mixture on a heat conducting surface so that said mixture forms a layer having a thickness between about 120 and about 300 micro

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
US 4,374,665 AMagnetostrictive devices198355
US 4,402,770 AHard magnetic alloys of a transition metal and lanthanide1983102
US 4,409,043 AAmorphous transition metal-lanthanide alloys198343
US 4,533,408 APreparation of hard magnetic alloys of a transition metal and lanthanide198562
US 4,715,891 AMethod of preparing a magnetic material19878
US 4,753,675 AMethod of preparing a magnetic material198814
US 4,770,723 AMagnetic materials and permanent magnets1988195
US 4,792,368 AMagnetic materials and permanent magnets1988142
US 4,802,931 AHigh energy product rare earth-iron magnet alloys1989110
JP H01171209 AManufacture of permanent magnet—9
US 4,851,058 AHigh energy product rare earth-iron magnet alloys198969
US 4,867,785 AMethod of forming alloy particulates having controlled submicron crystallite size distributions198922
US 4,935,074 AMagnetic material comprising iron, boron and a rare earth metal199029
US 4,994,109 AMethod for producing permanent magnet alloy particles for use in producing bonded permanent magnets199119
US 5,071,493 ARare earth-iron-boron-based permanent magnet199116
US 5,116,434 AMethod of manufacturing, concentrating, and separating enhanced magnetic parameter material from other magnetic co-products199211
EP 0,542,529 A1Method of making alloy powders of the RE-Fe/Co-B-M-type and bonded magnets containing this alloy powder—19
JP H08264363 AManufacture of rare earth permanent magnet—22
US 5,597,425 ARare earth cast alloy permanent magnets and methods of preparation199717
US 6,019,859 AIron-based permanent magnets and their fabrication as well as iron-based permanent magnet alloy powders for permanent bonded magnets and iron-based bonded magnets200020
US 6,022,424 AAtomization methods for forming magnet powders200054

Non-Patent Literature (1)

  • Kanekiyo, H. et al.: "Thick FE3B/ND2FE14B Nanocomposite Permanent Magnet Flakes Prepared by Slow Quenching," Journal of Applied Physics, U.S., American Institute of Physics, New York, vol. 83, No. 11, Part 2, Jun. 1, 1998, pp. 6265-6267.