Method of fabricating a highly reliable gate oxide

277Forward Citations (#26096 Global)
12.0/yrCitation Velocity (#30506 Global)
18.47Citation PageRank (#381403 Global)
2Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An ultra-thin gate oxide layer of hafnium oxide (HfO 2 ) and a method of formation are disclosed. The ultra-thin gate oxide layer of hafnium oxide (HfO 2 ) is formed by a two-step process. A thin hafnium (Hf) film is first formed by thermal evaporation at a low substrate temperature, after which the thin hafnium film is radically oxidized using a krypton/oxygen (Kr/O 2 ) high-density plasma to form the ultra-thin gate oxide layer of hafnium oxide (HfO 2 ). The ultra-thin gate oxide layer of hafnium oxide (HfO 2 ) formed by the method of the present invention is thermally stable in contact with silicon and is resistive to impurity diffusion at the HfO 2 /silicon interface. The formation of the ultra-thin gate oxide layer of hafnium oxide (HfO 2 ) eliminates the need for a diffusion barrier layer, allows thickness uniformity of the field oxide on the isolation regions and, more importantly, preserves the atomically smooth surface of the silicon substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 277.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for forming a gate structure for a semiconductor device comprising the steps of: forming a hafnium layer on a semiconductor substrate by thermal evaporation at a temperature of about 150° C. to about 200° C.; converting said hafnium layer to a hafnium oxide layer by oxidizing said hafnium layer; and forming a conductive layer over said hafnium oxide layer.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein said hafnium layer is formed to a thickness of about 10 Angstroms to about 100 Angstroms.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein said hafnium layer is formed to a thickness of about 10 Angstroms to about 50 Angstroms.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • "Advantage of Radical Oxidation for Improving Reliability of Ultra-Thin Gate Oxide" by Yuji Saito, et al. 2000 IEEE pp. 176-177.
  • "High-Integrity Silicon Oxide Grown at Low-Temperature by Atomic Oxygen Generated in High-Density Krypton Plasma" by Yuji Saito, et al, Extended Abstracts of the 1999 International Conference on Solid State Device and Materials, Tokyo, 1999, pp. 152-153.
  • "Low-Temperature Growth of High-Integrity Silicon Oxide Films by Oxygen Radical Generated in High-Density Krypton Plasma" by Masaki Hirayama, et al, 1999 IEEE pp. 249-252.