Patents
US 6,511,560 B2#15596393 Most CitedExpiredUnited States (USPTO)Utility

Thin, forged magnesium alloy casing and method for producing same

7Forward Citations (#15596393 Global)
0.3/yrCitation Velocity (#25562187 Global)
1.62Citation PageRank (#20286181 Global)
13Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A thin, forged magnesium alloy casing is integrally constituted by a thin plate with projections on either or both surfaces, and the thin plate is as thin as about 1.5 mm or less. The thin forged casing can be produced by (a) carrying out a first forging step for roughly forging a magnesium alloy plate to form an intermediate forged product under the conditions of a preheating temperature of the magnesium alloy plate of 350-500° C., a die temperature of 350-450° C., a compression pressure of 3-30 tons/cm 2 , a compressing speed of 10-500 mm/sec. and a compression ratio of 75% or less; and (b) carrying out a second forging step for precisely forging the intermediate forged product under the conditions of a preheating temperature of the intermediate forged product of 300-500° C., a die temperature of 300-400° C., a compression pressure of 1-20 tons/cm 2 , a compressing speed of 1-200 mm/sec., and a compression ratio of 30% or less.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for producing a thin, forged magnesium alloy product comprising carrying out forging by at least two steps, a first forging step being to roughly forge a magnesium alloy body preheated at 350-500° C. with a first die heated at 350-450° C. to form an intermediate forged product; and a second forging step being to precisely forge said intermediate forged product preheated at 300-500° C. with a second die heated at 300-400° C.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein said thin forged product is further subjected to a surface treatment selected from the group consisting of an anodic oxidation treatment and a paint coating.

  3. Claim 3Depends on #2

    The method according to claim 2 , wherein said surface treatment is an anodic oxidation treatment to keep metallic glow thereof.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • Database WPI, Section Ch, Week 198201, Derwent Publications Ltd., London, GB, AN 1982-01349E XP002161652 & SU 816 643 A (UFA Aviation Inst), Mar. 30, 1989 (abstract).
  • Database WPI, Section Ch, Week 199207, Derwent Publications Ltd., London, GB, AN 1992-051897 XP002161653 & JP 03 294036 A (Kobe Steel Ltd), Dec. 25, 1991 (abstract).
  • Naoki Osada (Graduate School of Industrial Technology, Nihon University); Mototsuga Katsuta (College of Industrial Technology, Nihon University), "Deep Drawability of AZ31 Magnesium Alloy Sheet", The 89th Autumn Convention of the Light Alloy Association in 1994, pp. 179-180.