Elimination of pad glazing for Al CMP
Abstract
Polishing pad glazing during CMP of Al and Al alloys is eliminated or substantially reduced by utilizing a neutral polishing slurry containing a sufficient amount of a surfactant to prevent agglomeration of the abrasive particles with polishing by-products. Embodiments include CMP an Al or an Al alloy surface employing a slurry containing abrasive Al 2 0 3 particles and about 0.02 to about 5 wt. % of a surfactant to prevent Al 2 0 3 abrasive slurry particles from agglomerating with Al(OH) 3 polishing by-products. Embodiments further include subsequent ex situ pad conditioning using an acid or base to dissolve, or a complexing agent to remove, Al(OH) 3 polishing by-products.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 13.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of planarizing an aluminum (Al) or Al alloy surface, the method comprising: chemical mechanical polishing (CMP) the surface with a polishing pad employing a slurry having a substantially neutral pH and containing abrasive alumina (Al 2 0 3 ) particles and a surfactant in an amount sufficient to prevent the Al 2 0 3 particles from agglomerating with aluminum hydroxide (Al(OH) 3 )-containing CMP by-products; and conditioning a polishing pad surface by treating the polishing pad surface with a chemical agent consisting essentially of a complexing agent capable of binding with (Al(OH) 3
- Claim 2Depends on #1
The method according to claim 1 , wherein the polishing pad surface is conditioned ex situ.
- Claim 3Depends on #1
The method according to claim 1 , wherein the chemical agent has a pH of a
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗