Method for removing contaminants from a semiconductor wafer

16Forward Citations (#5721040 Global)
0.7/yrCitation Velocity (#10886614 Global)
3.17Citation PageRank (#6929590 Global)
16Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for removing contaminants from a semiconductor wafer having a spin on coating of material. Contaminants are removed by applying a cleaning solution to the periphery, and preferably, the exposed backside of the wafer after the edge bead has been dissolved and removed. The cleaning solution is formulated to react chemically with unwanted coating material residue to form a compound that may be ejected from the periphery of the spinning wafer. Any residual solution or precipitate that is not ejected from the wafer may be rinsed away with water, preferably deoinized water. One exemplary use of this method is the removal of metallic contaminants that may be left on the periphery and backside of a wafer after the formation of ferroelectric film coatings. A cleaning solution comprising a mixture of hydrochloric acid HCl and water H 2 O or,ammonium hydroxide NH 4 OH and water H 2 O is applied to the periphery of the spinning wafer. The cleaning solution will react with any residual metal ions to form a metal chloride or metal hydroxide that is ejected from the wafer along with the cleaning solution.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 16.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for the manufacture of a semiconductor wafer, comprising the steps of: applying a ferroelectric coating material to a top surface of the semiconductor wafer; spinning the wafer; applying a solvent in which the coating material is soluble to the periphery of the spinning wafer; applying a cleaning solution to the periphery of the spinning wafer; and then rinsing the periphery of the wafer with water.

  2. Claim 2Independent Claim

    A method of processing a ferroelectric random access memory, comprising the steps of: applying a combination of metallic elements including a selection of strontium, bismuth, and tantalum to the top surface of a semiconductor wafer; spinning the wafer to form a metallic film on the wafer; applying a solvent in which the metallic film is soluble to the periphery o