US 6,506,676 B2#405076 Most CitedExpiredUnited States (USPTO)Utility

Method of manufacturing semiconductor devices with titanium aluminum nitride work function

77Forward Citations (#405076 Global)
3.4/yrCitation Velocity (#698125 Global)
11.94Citation PageRank (#791145 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of manufacturing semiconductor devices forms a surface channel CMOSFET in the process of manufacturing a metal gate. The method forms a (Ti x Al y ) 1-z N z film (where z ranges from about 0.0 to about 0.2) having a work function value ranging from about 4.2 to about 4.3 eV on a gate insulating film in a nMOS region, a (Ti x Al y ) 1-z N z film (where z ranges from about 0.3 to about 0.6) having a work function value ranging from about 4.8 to about 5.0 eV on the gate insulating film in a pMOS region, thus implementing a surface channel CMOS device both in the nMOS region and the pMOS region. Therefore, the threshold voltage is reduced.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 77.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing semiconductor devices comprising: forming a P-well and a N-well in a semiconductor substrate to define an nMOS region and a pMOS, respectively; forming a first gate insulating film in said nMOS region and a second gate insulating film in said pMOS region, respectively; forming a first (Ti x Al y ) 1 - z N z film on said first gate insulating film wherein “z” in said first (Ti x Al y ) 1 - z N z film ranges from about 0.0 to about 0.2 and a second (Ti x Al y ) 1 - z N z film on said second gate insulating film, respectively wherein “z” in said second (Ti x Al y ) 1

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 77 total)

PatentTitleYearCitations
US 2010024732 A1Systems for Flash Heating in Atomic Layer Deposition—38
US 7,122,414 B2Method to fabricate dual metal CMOS devices200626
US 2005104112 A1Method of depositing barrier layer from metal gates—52
US 2008102613 A1Controlled composition using plasma-enhanced atomic layer deposition—39
US 9,646,820 B2Methods for forming conductive titanium oxide thin films20173
US 2007259111 A1Method and apparatus for photo-excitation of chemicals for atomic layer deposition of dielectric film—43
US 9,523,148 B1Process for deposition of titanium oxynitride for use in integrated circuit fabrication201612
US 7,863,126 B2Fabrication of a CMOS structure with a high-k dielectric layer oxidizing an aluminum layer in PFET region201121
US 7,439,128 B2Method of creating deep trench capacitor using a P+ metal electrode20085
DE 112011100788 B4Elektrisches Bauelement, insbesondere CMOS-Bauelement, und Verfahren zum Herstellen eines Halbleiterbauelements20147
US 2009214767 A1Doping with ald technology—14
US 2022157600 A1Film forming method, method for manufacturing semiconductor device, film forming device, and system for manufacturing semiconductor device—2
US 12,119,219 B2Film forming method, method for manufacturing semiconductor device, film forming device, and system for manufacturing semiconductor device20240
US 7,785,958 B2Method for making a semiconductor device having a high-k gate dielectric layer and a metal gate electrode201025
US 7,732,872 B2Integration scheme for multiple metal gate work function structures201021

Non-Patent Literature (2)

  • Kim et al., "Anti oxidation properties of TiAIN film prepared by plasma assisted CVD and roles of AI", Thin Solid Film 307, 1997, pp. 113-119.
  • Shew et al., "Effects of RF bias and nitrogen flow rates on the reactive sputtering of TiAIN films", Thin Solid Films 293, 1997, pp. 212-219.*