Patents
US 6,506,231 B2#4341960 Most CitedExpiredUnited States (USPTO)Utility

Method and apparatus for making metallic iron

20Forward Citations (#4341960 Global)
0.9/yrCitation Velocity (#8341191 Global)
2.11Citation PageRank (#13308757 Global)
22Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of making metallic iron in which a compact, containing iron oxide such as iron ore or the like and a carbonaceous reductant such as coal or the like, is used as material, and the iron oxide is reduced through the application of heat, thereby making metallic iron. In the course of this reduction, a shell composed of metallic iron is generated and grown on the surface of the compact, and slag aggregates inside the shell. This reduction continues until substantially no iron oxide is present within the metallic iron shell. Subsequently, heating is further performed to melt the metallic iron and slag. Molten metallic iron and molten slag are separated one from the other, thereby obtaining metallic iron with a relatively high metallization ratio. Through the employment of an apparatus for making metallic iron of the present invention, the above-described method is efficiently carried out, and metallic iron having a high iron purity can be made continuously as well as productively not only from iron oxide having a high iron content but also from iron oxide having a relatively low iron content.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 20.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for producing metallic iron, comprising the steps of: (A) heating a mixture comprising an iron oxide and a carbonaceous reducing agent; (B) reducing said iron oxide of said mixture; (C) producing a metallic iron and a liquid slag from said mixture by said heating and reducing, where said metallic iron forms at least one metallic iron shell surrounding a cavity and where at least a portion of said slag is within said cavity; (D) melting at least part of said metallic iron; and (E) separating said slag from said metallic iron.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein during said melting said metallic iron is carburized by said carbonaceous reducing agent.

  3. Claim 3Depends on #2

    The method of claim 2 , further comprising a step of chilling said metallic iron, thereby forming a granula

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗