Surface-treated aluminum material with superior adhesive properties and production method therefor
Abstract
The present invention relates to an aluminum material to which a surface treatment is performed, and has as its objective the provision of a surface-treated aluminum material that has excellent adhesive properties with organic resin film. The present invention further aims to provide a method for producing the aforementioned. In the present invention's surface-treated aluminum material, a non-porous anodic oxide film is formed to the surface of the aluminum or aluminum alloy. This non-porous anodic oxide film has a thickness in the range of 5˜800 nm, a porosity of 20% or less, and contains in an amount of 50 ppm or more at least one of silicon, phosphorous, boron or carbon as a component. As a result of this structure, the adhesive properties between organic resin film and non-porous anodic oxide film can be increased. Further, if the present invention's surface-treated aluminum material to which an organic resin film has been laminated is employed in various containers such as beverage cans, or in decorative boards used in furniture or interior construction materials, peeling will not occur when the material is subjected to further working. Moreover, corrosion does not occ
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 24.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A surface-treated aluminum material, comprising a non-porous anodic oxide film formed at the surface of an aluminum or an aluminum alloy, wherein the thickness of the non-porous anodic oxide film is in the range of 5˜800 nm, the porosity of the non-porous anodic oxide film is at most 20%, and the surface-treated aluminum material contains at least 50 ppm of at least one member selected from the group consisting of silicon, phosphorus, boron, and carbon.
- Claim 2Depends on #1
The surface-treated aluminum material according to claim 1 , wherein the non-porous anodic oxide film contains at least 50 ppm of at least one member selected from the group consisting of silicon and phosphorus.
- Claim 3Depends on #2
The surface-treated aluminum material according to claim 2 , wherein the non-porous anodic oxide film contains from 100 to 20,000 ppm of silicon.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 24 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,859,288 A | Porous anodic aluminum oxide films | 1989 | 40 |
| US 5,131,987 A | Process for making an adhesively bonded aluminum article | 1992 | 16 |