Single crystal silicon layer, its epitaxial growth method and semiconductor device
Abstract
In case of epitaxially growing a single crystal silicon layer by catalytic CVD on a material layer in lattice alignment with single crystal silicon, i.e. a substrate of single crystal silicon, sapphire, spinel, or the like, the total pressure of the growth atmosphere is maintained in the range from 1.33×10 −3 Pa to 4 Pa at least in the initial period of the epitaxial growth, or alternatively, partial pressure of oxygen and moisture in the growth atmosphere is maintained in the range from 6.65×10 −10 to 2×10 −6 Pa at least in the initial period of the epitaxial growth. Thus, the maximum oxygen concentration of the epitaxially grown single crystal silicon layer becomes not higher than 3×10 18 atoms/cm −3 at least in a portion with the thickness of 10 nm from the boundary with the substrate 4. It is thus ensured to epitaxially grow a high-quality single crystal silicon layer at a lower temperature than that of existing CVD.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A single crystal silicon layer epitaxially grown by catalytic CVD on a material layer in lattice alignment with single crystal silicon, characterized in: a maximum oxygen concentration thereof being not higher than 3×10 18 atoms/cm 3 at least in a region having the thickness of 10 nm thick from the boundary between said material layer and said single crystal silicon layer.
- Claim 2Depends on #1
The single crystal silicon layer according to claim 1 wherein the maximum oxygen concentration thereof is not higher than 2×10 18 atoms/cm 3 at least in a region having the thickness of 10 nm from the boundary between said material layer and said single crystal silicon layer.
- Claim 3Depends on #1
The single crystal silicon layer according to claim 1 wherein the maximum oxygen concentration thereof is not higher than 3×10 18 atoms/cm 3 at
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 5,814,149 A | Methods for manufacturing monocrystalline diamond films | 1998 | 57 |
| US 6,204,518 B1 | SRAM cell and its fabrication process | 2001 | 21 |