Lead-acid battery having tin in positive active material and silica in separator
Abstract
In a lead-acid battery, a positive active material includes tin in an amount of from not less than 0.2% to not more than 5% based on the weight thereof. The density of the positive active material after formation is from not less than 3.75 g/cc to not more than 5.0 g/cc. When the lead-acid battery is produced by a battery container formation, a time required between the injection of an electrolyte and the beginning of battery container formation is from not less than 0.1 hours to not more than 3 hours.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 9.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A lead-acid battery comprising an electrolyte and a positive active material including tin in an amount of from not less than 0.5% to not more than 5% based on the weight thereof; wherein the density of said positive active material after formation is from not less than 3.75 g/cc to not more than 5.0 g/cc; wherein said led-acid battery is a valve-regulated lead-acid battery; wherein said lead-acid battery comprises a fine glass fiber separator containing a powdered silica having a specific surface area of from 50 to 500 m 2 /g added therein in an amount of weight not less than 30% to not more
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (5)
Non-Patent Literature (3)
- Patent Abstracts of Japan, vol. 016, No. 166 (E-1193), Apr. 22, 1992 for JP-A-4-14758.
- Patent Abstracts of Japan, vol. 017, No. 353 (E-1393), Jul. 5, 1993 for JP-A-5-54881.
- Patent Abstracts of Japan, vol. 096, No. 011, Nov. 29, 1996 for JP-A-8-180876.