Abstract
The inventive method comprises compressing roughly half a bun of polyimide foam at a rate of no more than 12 feet per minute from its initial height of approximately 15″, until it reaches a compressed height of no more than 2″. The compression is maintained on the bun for no more than one minute, and then released. The half-bun is then permitted to expand, and it will rebound to approximately 90-95% of its initial height. This conditioned foam may then be cut or otherwise formed into acoustical panels of varying heights and/or configurations, without worry about the ultimate shrinkage after treatment. In addition the treated half-bun may be cut into irregular shapes of more varying dimensions, up to the maximum dimension of the treated half-bun.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 1.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of treating a piece of cured foamed material, said piece having a top, bottom and sides, and a height measured between said top and said bottom thereof, said method comprising: compressing said piece at a rate of no more than twelve feet per minute; stopping said compressing when said piece is compressed to no more than 15% of said height; maintaining pressure on said piece for a period of no more than one minute after compression of said piece stops; releasing said pressure on said piece; and permitting said piece to rebound for a period of no less than 48 hours, whereby the acoustic
- Claim 2Depends on #1
The method of claim 1 , wherein said compressing is performed at a rate of no more than approximately five feet per minute.
- Claim 3Independent Claim
The m