US 6,489,649 B2#944877 Most CitedExpiredUnited States (USPTO)Utility

Semiconductor device having nonvolatile memory and method of manufacturing thereof

50Forward Citations (#944877 Global)
2.1/yrCitation Velocity (#1889728 Global)
5.14Citation PageRank (#3171925 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Described is a semiconductor device having a silicon oxide (SiO2) film into which nitrogen atoms, in a range between approximately 2x1020 atoms/cm3 or more and 2x1021 atoms/cm3 or less, are introduced, used as an insulator film in the semiconductor device. For example, the device can be a nonvolatile memory device, and the silicon oxide film can be used as an insulator film between, e.g., a floating gate electrode and control gate electrode of the nonvolatile memory device. Stable operations and a retention capability of a nonvolatile memory device are obtained even if the nonvolatile memory device is scaled. Moreover, a programming voltage can be lowered. Also described are methods of fabricating the semiconductor device.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 50.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A semiconductor device having a nonvolatile memory, the nonvolatile memory comprising a silicon oxide film formed between a first silicon film which is a floating gate and a second silicon film which is a control gate, the first silicon film overlying a substrate, the silicon oxide film having a thickness in a direction from the first silicon film to the second silicon film, and extends from adjacent the first silicon film to adjacent the second silicon film, the silicon oxide film having nitrogen included therein in an entirety of the thickness thereof, a maximum nitrogen concentration in the

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 50 total)

Non-Patent Literature (5)

  • "Electrical and Physical Characteristics of Thiim Nitrided Oxides Prepared by Rapid Thermal Nitridation", Hori, et al., vol. ED-34, No. 11, Nov. 1987.
  • "Hydrogen in low-pressure chemical-vapor-deposited silicon (oxy)nitride films", Habraken, et al., J. Appl. Phys. 59(2), Jan. 15, 1986, pp. 447-453.
  • "ONO Inter-Poly Dielectric Scaing for Nonvolatile Memory Applications", Mori, et al., vol. 38, No. 2 Feb. 1991.
  • "Reduced Poly-Si TFT Threshold Voltage Instability by High-Temperature Hydrogenation of a-Si-Like Spin Centers", Kamigaki, et al., pp. 12-17.
  • Nakayama "AP+Poly-Si Gate with Nitrogen-Doped Poly-Si Layer for Deep Submicron PMOSFETS", Pennington, NJ, USA: Electrochem. Soc, p. 9-16, May 1991.*