Abstract

The present invention provides a manufacturing method of copolyester for low acetaldehyde content of PET bottles. The polyethylene terephthalate (PET) polymer is added with an appropriate modifier in order to decrease the production of acetaldehyde caused by pyrolysis side reaction during the blow molding process of PET bottles. The modifier comprises stabilizer and primary antioxidant, wherein the stabilizer is an inorganic phosphorous compound with an addition quantity of 0.003˜0.5 weight % based on the weight of the total copolyester copolymer and the primary antioxidant is a hindered phenolic antioxidant containing Ca +2 with an addition quantity of 0.005˜5.0 weight % based on the weight of the total copolyester copolymer. The present invention owns an improving effect of decreasing the production of side product—acetaldehyde at least 30% than those without the addition of said modifier.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 21.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A manufacturing method of copolyester for low acetaldehyde content of PET bottles, whose characteristic is to add 0˜10 mole % isophthalic acid into the dicarboxyl acid component and the dihydric alcohol component repeat unit so as to have the dicarboxyl acid component and the dihydric alcohol component complete over 95% of esterification conversion ratio; the catalyst, stabilizer, toner, and hindered phenolic antioxidant having a structure containing calcium and phosphorous elements, wherein the calcium element is in the amount of 2-200 ppm based on the weight of the polyester, are then added

  2. Claim 2Depends on #1

    A manufacturing method of copolyester for low acetaldehyde content of PET bottles as defined in claim 1 , wherein at least 80 mole % is terephthalic acid or 2,6-naphthalenedi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 21 total)

PatentTitleYearCitations
US 2006002867 A1UV barrier formulation for polyesters—3
WO 2006/138406 A3High intrinsic viscosity melt phase polyester polymers with acceptable acetaldehyde generation rates—0
US 2011190470 A1Synthesis of polyesters with precisely sequenced two or more structural units—3
US 9,006,382 B2Synthesis polyesters with precisely sequenced two or more structural units20150
US 2006258786 A1Method to reduce the aldehyde content of polymers—2
US 2007129501 A1Manufacturing method of co-polyester resins for clear mono-layer containers with improved gas barrier characteristics—14
US 2005239938 A1Metal phosphonates and related nanocomposites—12
US 2004058805 A1Polymerization catalyst for polyester, polyester produced with the same, and process for producing polyester—38
US 8,530,612 B2Synthesis of polyesters with precisely sequenced two or more structural units20130
US 7,763,265 B2UV barrier formulation for polyesters20102
US 2007066791 A1Aluminum containing polyester polymers having low acetaldehyde generation rates—23
US 2003045673 A1Polymerization catalyst for polyesters, polyesters produced with the same and process for producing polyesters—25
US 2009186177 A1Polyester melt phase products and process for making the same—3
US 7,358,324 B2Manufacturing method of co-polyester resins for clear mono-layer containers with improved gas barrier characteristics200824
CN 101,198,634 BHigh intrinsic viscosity melt phase polyester polymers with acceptable acetaldehyde generation20110