Process for synthesizing trans-1,4-polybutadiene
Abstract
The process and catalyst system of this invention can be utilized to synthesize polybutadiene rubber having a high trans content and a low melting point by solution polymerization. The trans-polybutadiene rubber made by the process of this invention can be utilized in tire tread rubbers that exhibit outstanding wear characteristics. More importantly, the trans-polybutadiene rubber of this invention can be easily processed because of its low level of crystallinity. In fact, the trans-polybutadiene made by the process of this invention does not need to be heated in a “hot-house” before being used in making rubber compounds. This invention more specifically reveals a process for synthesizing trans-polybutadiene rubber which comprises polymerizing 1,3-butadiene in an organic solvent in the presence of a catalyst system which comprises (a) an organolithium compound, (b) a barium compound selected from the group consisting of (i) barium salts of cyclic alcohols, such as barium mentholate, and (ii) barium thymolate, and (c) an organoaluminum compound. The trans-polybutadiene made with the catalyst system of this invention typically has a glass transition temperature that is within the ran
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 27.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for synthesizing trans-1,4-polybutadiene which comprises polymerizing 1,3-butadiene monomer in the presence of a catalyst system which is comprised of (a) an organolithium compound, (b) a barium compound selected from the group consisting of (i) a barium salt of a di-alkylated cyclohexanol, and (ii) barium thymolate, and (c) an orgnoaluminum compound.
- Claim 2Depends on #1
A process as specified in claim 1 wherein the polymerization temperature is within the range of about 20° C. to about 120° C.
- Claim 3Depends on #1
A process as specified in claim 1 wherein the polymerization temperature is within the range of about 40° C. to about 100° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 27 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 5,086,136 A | Process for producing high trans low vinyl conjugated diene (co)polymer | 1992 | 41 |
| US 5,100,965 A | Process for synthesizing high trans polymers | 1992 | 55 |