Patents
US 6,479,170 B2#22372336 Most CitedExpiredUnited States (USPTO)Utility

Electrodeposited copper foil, method of inspecting physical properties thereof, and copper-clad laminate employing the electrodeposited copper foil

5Forward Citations (#22372336 Global)
0.2/yrCitation Velocity (#32394499 Global)
1.15Citation PageRank (#34133666 Global)
2Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention provides an electrodeposited copper foil which solves problems of electrodeposited-copper-clad laminates to which the foil has been incorporated, such as bow, twist, and poor dimensional stability, and a method of inspecting an electrodeposited copper foil so as to assure the quality of the foil. In the invention, there is employed an electrodeposited copper foil which recrystallizes by heating at low temperature during production of a copper-clad laminate employing an electrodeposited copper foil and which exhibits an elongation as high as 18% or more in an atmosphere of 180° C., wherein the maximum rate of decrease in maximum tensile strength falls within the aging time ranging from 5 to 10 minutes in a process in which tensile strength decreases as time elapses during aging in an atmosphere at 170° C., and the change in tensile strength in a knick portion shown in a {tensile strength} vs. {aging time} curve which is drawn in an x-y plane and which has a knick portion is 3 kg/mm2 or more, the x-axis representing aging time and the y-axis representing tensile strength.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 5.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An electrodeposited copper foil providing improved bow and twist and dimensional stability to copper-clad laminates which: recrystallizes by heating at low temperature during production of a copper-clad laminate employing an electrodeposited copper foil; and exhibits an elongation as high as 18% or more in an atmosphere at 180° C., comprising selecting those copper foils wherein the maximum rate of decrease in maximum tensile strength falls within an aging time ranging from 5 to 10 minutes during aging in an atmosphere at 170° C., and the change in tensile strength in a knick portion shown in

  2. Claim 2Depends on #1

    A method of selecting an electrodeposited copper foil of claim 1 , comprising cutting an electrodeposit copper foil and prepar

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗