Abstract

A semiconductor ceramic having a negative temperature coefficient of resistance, the element comprising about 0.1 to 20 mol % of AMnO 3 (A represents at least one of Ca, Sr, Ba, La, Pr, Nd, Sm, Eu, Gd, Tb, Dy and Ho) and to a spinel composite oxide made of a solid solution of Mn and at least one element in Ti, V, Cr, Fe, Co, Ni, Cu, Zn, Mg and Al. As a perovskite Mn composite oxide, one or more of CaMnO 3 , SrMnO 3 , BaMnO 3 , LaMnO 3 , PrMnO 3 , NdMnO 3 , SmMnO 3 , EuMnO 3 , GdMnO 3 , TbMnO 3 , DyMnO 3 and HoMnO 3 may be used.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 20.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A semiconductor ceramic having a negative temperature coefficient of resistance, comprising: a spinel composite oxide comprising a solid solution of Mn and at least one element selected from the group consisting of Ti, V, Cr, Fe, Co, Ni, Cu, Zn, Mg and Al; and about 0.1 to 20 mol % of AMnO 3 , wherein A is at least one member selected from the group consisting of Ca, Sr, Ba, La, Pr, Nd, Sm, Eu, Gd, Tb, Dy and Ho.

  2. Claim 2Depends on #1

    A semiconductor ceramic having a negative temperature coefficient of resistance according to claim 1 , wherein the spinel composite oxide comprises a solid solution of Mn and at least one element selected from the group consisting of Fe, Co, Ni and Al; and A represents at least one member of the group consisting of Ca, Sr, Ba and La.

  3. Claim 3Independent Claim

    A semiconductor ceramic ha

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 20 total)

PatentTitleYearCitations
US 7,548,149 B2Surface-mount negative-characteristic thermistor20095
US 2019077677 A1Ceramic material and resistive element—2
US 6,878,311 B2Ceramic mixture having negative temperature co-efficient, a thermistor containing the ceramic mixture and a process for preparing same20050
US 2011031451 A1Sintered body, and thermoelectric conversion material—1
US 2004164280 A1Ceramic mixture having negative temperature co-efficient, a thermistor containing the ceramic mixture and a process for preparing same—4
US 9,341,521 B2Composite material for temperature measurement, temperature sensor comprising the composite material, and method for producing the composite material and the temperature sensor20162
US 2008048821 A1Surface-mount negative-characteristic thermistor—15
US 10,446,298 B2Method for producing an electrical component20190
US 9,337,497 B2Layer structure and use thereof to form a ceramic layer structure between an interconnect and a cathode of a high-temperature fuel cell20160
US 2004020918 A1Negative temperature coefficient thermistor and method for manufacturing the same—4
US 2010134237 A1Semi-conductive ceramic material and ntc thermistor using the same—7
US 10,364,161 B2Ceramic material and resistive element20193
US 2012200969 A1Resistive Element, Infrared Light Sensor, and Electrical Device—7
CN 100,541,674 CThe ceramic mixture and its preparation method that are used for the negative temperature coefficient of thermistor20091
US 6,861,622 B2Negative temperature coefficient thermistor and method for manufacturing the same20052