Patents
US 6,468,658 B2#15196264 Most CitedExpiredUnited States (USPTO)Utility

Process for preparing grit blasting particles coated with titanium dioxide

7Forward Citations (#15196264 Global)
0.3/yrCitation Velocity (#26083970 Global)
1.79Citation PageRank (#17373115 Global)
3Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A process for preparing grit blasting particles coated with titanium dioxide by sinter-fusing titanium dioxide on the surface of grit blasting particles made of a base material. A mixture of finely divided titanium dioxide and grit blasting particles is passed continuously through the flame in a flame reactor, with the aid of conveying air, wherein the titanium dioxide is sinter-fused on the surface of the grit blasting particles over an average residence time of 0.1 to 5 seconds in a temperature range from 600 to 1200° C. An increase in the adhesive bond between metal framework and a facing material made of plastics in dentures can be achieved when metal framework is grit blasted with a grit blasting agent containing titanium dioxide coated grit blasting particles and then the grit blasted and titanium dioxide coated surface is treated with a silane bonding agent.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for preparing grit blasting particles coated with titanium dioxide comprising sinter-fusing titanium dioxide on the surface of grit blasting particles made of a base material, by continuously passing a mixture of finely divided titanium dioxide and grit blasting particles through a flame in a flame reactor, in a stream of conveying air, and sinter-fusing titanium dioxide on the surface of the grit blasting particles over an average residence time of 0.1 to 5 seconds in a temperature range from 600 to 1200° C.

  2. Claim 2Depends on #1

    The process according to claim 1 , wherein the mixture is blown at a rate of 1 to 50 m/s, with conveying air, centrally into a ring flame operated with fuel gas.

  3. Claim 3Depends on #1

    The process according to claim 1 , wherein the grit blasting particles consist of a ceramic material, glass or metal as the base material

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Copy of German Office Action in counterpart appln. No. 100 29 598.3, dated May 21, 2001.